M35 Tool Die Steels

M35 - Specification & Application

High-Speed Tool Steel

Chemical composition(wt.%) of M35 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.80 0.85
Si 0.20 0.40
Mn 0.20 0.40
Cr 3.90 4.40
Mo 3.00 3.50
V 4.75 5.25
W 6.15 6.65
Co 4.75 5.25

M35 - Detail

High-Speed Tool Steel

Mechanical properties of grade M35

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
329 (≥) 522 (≥) 34 14 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade M35

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
683 (≥) 844 (≥) 14 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
367 173 626

Equivalent Products

We can customize the production of M35 grade, contact us for the best solution.