Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
Ni | 63.00 | - | ||
Mn | - | 2.00 | ||
S | - | 0.50 | ||
Cu | 28.00 | 34.00 | ||
C | - | 0.30 | ||
Fe | - | 2.50 | ||
Si | - | 0.024 |
A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media, including sea water, hydrofluoric acid,sulfuric acid and alkalies. Used for marine engineering, chemical and hydrocarbon processing equipment, valves, pumps, shafts,fittings, fasteners and heat exchangers
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
924 (≥) | 463 (≥) | 34 | 24 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 212 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
272 (≥) | 136 (≥) | 33 | 12 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 343 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
333 | 143 | 588 |
We can customize the production of MONEL ALLOY 400 grade, contact us for the best solution.