NCF 751 Stainless Steels to G 4902 (1991)

NCF 751 - Specification & Application

  • G 4902 (1991) - Corrosion-resisting and heat-resisting superalloy plates and sheets

Corrosion-resisting and heat-resisting superalloy plates and sheets

Chemical composition(wt.%) of NCF 751 grade: to G 4902 (1991)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.50
Mn - 1.00
P - 0.03
S - 0.015
Cr 14.00 17.00
Ni 70.00 -
Cu - 0.50
Al 0.90 1.50
Ti 2.00 2.60
Fe 5.00 9.00
Nb+Ta 0.70 1.20

NCF 751 - Detail

Corrosion-resisting and heat-resisting superalloy plates and sheets

Mechanical properties of grade NCF 751 G 4902 (1991)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
496 (≥) 742 (≥) 41 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade NCF 751 G 4902 (1991)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
518 (≥) 274 (≥) 14 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 211
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
427 362 366

Equivalent Grade

Equivalent Products

We can customize the production of NCF 751 grade, contact us for the best solution.