NCF600TB Stainless Steels to D 3757 (2003)

NCF600TB - Specification & Application

  • D 3757 (2003) - Seamless nickel-chromium-iron alloy heat exchanger tubes

Seamless nickel-chromium-iron alloy heat exchanger tubes

Chemical composition(wt.%) of NCF600TB grade: to D 3757 (2003)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 0.50
Mn - 1.00
P - 0.030
S - 0.015
Cr 14.00 17.00
Ni 72.00 -
Cu - 0.50
Al - -
Ti - -
Fe 6.00 10.00

NCF600TB - Detail

Seamless nickel-chromium-iron alloy heat exchanger tubes

Mechanical properties of grade NCF600TB D 3757 (2003)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
887 (≥) 232 (≥) 24 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade NCF600TB D 3757 (2003)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
184 (≥) 722 (≥) 44 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
865 397 957

Equivalent Products

We can customize the production of NCF600TB grade, contact us for the best solution.