Ni-Mo28 Stainless Steels to NF A 54-401

Ni-Mo28 - Specification & Application

  • NF A 54-401 - Nickel and nickel alloys. Nickel-molybdenum and nickel-molybdenum- chromium-alloys

Nickel and nickel alloys. Nickel-molybdenum and nickel-molybdenum- chromium-alloys

Chemical composition(wt.%) of Ni-Mo28 grade: to NF A 54-401

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 1.00
Mn - 1.00
P - 0.025
S - 0.030
Cr - 1.00
Ni - remaining
Mo 26.00 30.00
V 0.20 0.40
Co - 2.50

Ni-Mo28 - Detail

Nickel and nickel alloys. Nickel-molybdenum and nickel-molybdenum- chromium-alloys

Mechanical properties of grade Ni-Mo28 NF A 54-401

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
783 (≥) 991 (≥) 31 12 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade Ni-Mo28 NF A 54-401

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
264 (≥) 784 (≥) 11 12 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
237 518 148

Equivalent Grade

Equivalent Products

We can customize the production of Ni-Mo28 grade, contact us for the best solution.