NiCr20TiAI Superalloys to NF EN 10269

NiCr20TiAI - Specification & Application

  • NF EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Chemical composition(wt.%) of NiCr20TiAI grade: to NF EN 10269

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 1.00
P - 0.020
S - 0.015
Cr 18.00 21.00
Ni 65.00 -
Mo - -
Ti 1.80 2.70
Co 0.60 0.80
Al 1.00 1.80
Fe - 1.50
Cu - 0.20

NiCr20TiAI - Detail

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Mechanical properties of grade NiCr20TiAI NF EN 10269

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
158 (≥) 829 (≥) 41 13 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade NiCr20TiAI NF EN 10269

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
752 (≥) 729 (≥) 24 44 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 331
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
637 778 618

Equivalent Products

We can customize the production of NiCr20TiAI grade, contact us for the best solution.