Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.04 | 0.10 | ||
Si | - | 1.00 | ||
Mn | - | 1.00 | ||
P | - | 0.020 | ||
S | - | 0.015 | ||
Cr | 18.00 | 21.00 | ||
Mo | - | - | ||
Ni | 65.00 | - | ||
Al | 1.00 | 1.80 | ||
Fe | - | 3.00 | ||
Co | - | 2.00 | ||
B | - | 0.008 | ||
Cu | - | 0.20 | ||
Ti | 1.80 | 2.70 |
Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
868 (≥) | 684 (≥) | 32 | 41 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
343 (≥) | 889 (≥) | 14 | 41 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 242 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
467 | 176 | 725 |
We can customize the production of NiCr20TiAl grade, contact us for the best solution.