R30155 Stainless Steels

R30155 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of R30155 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 -
Si 0.50 -
Mn 1.50 -
P - -
S - -
Cr 21.3 -
Ni 20.0 -
Mo 3.00 -

R30155 - Detail

Steel for exhaust valves

Mechanical properties of grade R30155

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
422 (≥) 162 (≥) 33 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade R30155

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
553 (≥) 786 (≥) 41 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 222
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
876 341 685

Equivalent Products

We can customize the production of R30155 grade, contact us for the best solution.
sales@specificsteel.com