RA 330 Stainless Steels to SAE J 470 (1976)

RA 330 - Specification & Application

  • SAE J 470 (1976) - Wrought nickel and nickel-related alloys

Wrought nickel and nickel-related alloys

Chemical composition(wt.%) of RA 330 grade: to SAE J 470 (1976)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 1.25
Mn - 1.00
Cr - 19.00
Ni - 35.00
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - remaining

RA 330 - Detail

Wrought nickel and nickel-related alloys

Mechanical properties of grade RA 330 SAE J 470 (1976)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
853 (≥) 248 (≥) 42 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade RA 330 SAE J 470 (1976)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
665 (≥) 537 (≥) 12 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
538 851 925

Equivalent Grade

Equivalent Products

We can customize the production of RA 330 grade, contact us for the best solution.