RA 333 Stainless Steels to SAE J 470 (1976)

RA 333 - Specification & Application

  • SAE J 470 (1976) - Wrought nickel and nickel-related alloys

Wrought nickel and nickel-related alloys

Chemical composition(wt.%) of RA 333 grade: to SAE J 470 (1976)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 1.15
Mn - 1.00
Cr - 25.50
Ni - remaining
Mo - 3.25
Co - 3.00
W - 3.25
Al - -
Cu - 0.10
Ti - -
Fe - 17.00

RA 333 - Detail

Wrought nickel and nickel-related alloys

Mechanical properties of grade RA 333 SAE J 470 (1976)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
124 (≥) 869 (≥) 11 12 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade RA 333 SAE J 470 (1976)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
725 (≥) 132 (≥) 23 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
873 649 393

Equivalent Products

We can customize the production of RA 333 grade, contact us for the best solution.