S31753 Stainless Steels

S31753 - Specification & Application

Austenitic Nitrogen-Bearing Stainless Steel

Chemical composition(wt.%) of S31753 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 1.00
P - 0.03
S - 0.03
Cr 18.00 20.00
Ni 11.00 15.00
Mo - -
N 0.10 0.22

S31753 - Detail

Austenitic Nitrogen-Bearing Stainless Steel

Mechanical properties of grade S31753

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
328 (≥) 399 (≥) 44 44 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade S31753

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
257 (≥) 882 (≥) 44 44 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 343
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
697 147 241

Equivalent Products

We can customize the production of S31753 grade, contact us for the best solution.