S44020 Stainless Steels

S44020 - Specification & Application

S44020

Chemical composition(wt.%) of S44020 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.95 1.2
Si - 1
Mn - 1.25
P - 0.04
S 0.1 0.35
Cr 16.0 18.0
Ni - 0.75
Mo 0.40 0.60
N - 0.08

S44020 - Detail

S44020

Mechanical properties of grade S44020

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
547 (≥) 244 (≥) 13 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade S44020

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
292 (≥) 598 (≥) 42 22 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
614 347 261

Equivalent Products

We can customize the production of S44020 grade, contact us for the best solution.