S44023

Chemical composition(wt.%) of S44023 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.95 1.2
Si - 1
Mn - 1.25
P - 0.04
S - 0.03
Cr 16.0 18.0
Ni - 0.75
Mo - 0.6
Se 0.15 -

S44023 - Detail

S44023

Mechanical properties of grade S44023

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
448 (≥) 579 (≥) 12 14 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade S44023

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
314 (≥) 619 (≥) 44 14 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
183 471 371

Equivalent Products