S63011 Stainless Steels

S63011 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of S63011 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.65 0.75
Si 0.45 0.85
Mn 5.50 7.00
P - 0.050
S 0.025 0.065
Cr 20.0 22.0
Ni 1.40 1.90
N 0.18 0.28

S63011 - Detail

Steel for exhaust valves

Mechanical properties of grade S63011

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
226 (≥) 185 (≥) 43 22 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade S63011

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
955 (≥) 445 (≥) 31 23 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
668 495 396