Seamless Austenitic Steel Pipe for High-Temperature Central-Station Service
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.045 | 0.10 | ||
Si | - | 0.75 | ||
Mn | - | 2.00 | ||
Cr | 14.5 | 16.5 | ||
Ni | 7.5 | 9.5 | ||
Mo | 1.50 | 2.00 |
Seamless Austenitic Steel Pipe for High-Temperature Central-Station Service
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
463 (≥) | 385 (≥) | 11 | 21 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
638 (≥) | 215 (≥) | 31 | 41 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 142 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
262 | 267 | 234 |
We can customize the production of SA-376 16-8-2H grade, contact us for the best solution.