STR1 Stainless Steels to D 3731 (2002)

STR1 - Specification & Application

  • D 3731 (2002) - Heat - resisting steel bars

Heat - resisting steel bars

Chemical composition(wt.%) of STR1 grade: to D 3731 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40 0.50
Si 3.00 3.50
Mn - 0.60
P - 0.03
S - 0.03
Cr 7.50 9.50
Ni - -
Mo - -
N - -
Cu - 0.30

STR1 - Detail

Heat - resisting steel bars

Mechanical properties of grade STR1 D 3731 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
557 (≥) 768 (≥) 22 21 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade STR1 D 3731 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
899 (≥) 949 (≥) 11 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
499 897 426

Equivalent Grade

Equivalent Products

We can customize the production of STR1 grade, contact us for the best solution.
sales@specificsteel.com