STR31 Stainless Steels to D 3731 (2002)

STR31 - Specification & Application

  • D 3731 (2002) - Heat - resisting steel bars

Heat - resisting steel bars

Chemical composition(wt.%) of STR31 grade: to D 3731 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.45
Si 1.50 2.50
Mn - 0.60
P - 0.040
S - 0.030
Cr 14.00 16.00
Ni 13.00 15.00
Mo - -
N - -
W 2.00 3.00

STR31 - Detail

Heat - resisting steel bars

Mechanical properties of grade STR31 D 3731 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
464 (≥) 784 (≥) 22 44 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade STR31 D 3731 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
669 (≥) 492 (≥) 44 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
845 537 145

Equivalent Grade

Equivalent Products

We can customize the production of STR31 grade, contact us for the best solution.