STS321TP Stainless Steels to D 3576 (2011)

STS321TP - Specification & Application

  • D 3576 (2011) - Stainless steel pipes
  • D 9536 (2011) - Stainless lined steel pipe

Stainless lined steel pipe

Chemical composition(wt.%) of STS321TP grade: to D 3576 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 17.00 19.00
Ni 9.00 13.00
Mo - -
N - -
Ti 5×C% -

STS321TP - Detail

Stainless lined steel pipe

Mechanical properties of grade STS321TP D 3576 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
769 (≥) 245 (≥) 12 42 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade STS321TP D 3576 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
653 (≥) 592 (≥) 43 34 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
871 295 243

Equivalent Products