STS430J1L Stainless Steels to D 3698 (2008)

STS430J1L - Specification & Application

  • D 3698 (2008) - Cold rolled stainless steel plates, sheets and strip
  • D 3705 (2008) - Hot rolled stainless steel plates, sheets and strip

Hot rolled stainless steel plates, sheets and strip

Chemical composition(wt.%) of STS430J1L grade: to D 3698 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 16.00 20.00
Ni - 0.60
Mo - -
N - 0.025
Cu 0.30 0.80
Ti,Nb,Zr 8×(C%+N%) 0.80

STS430J1L - Detail

Hot rolled stainless steel plates, sheets and strip

Mechanical properties of grade STS430J1L D 3698 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
597 (≥) 289 (≥) 21 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade STS430J1L D 3698 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
448 (≥) 481 (≥) 43 44 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
712 714 721

Equivalent Grade

Equivalent Products

We can customize the production of STS430J1L grade, contact us for the best solution.