STSF316 Stainless Steels to D 4115 (2001)

STSF316 - Specification & Application

  • D 4115 (2001) - Stainless steel forgings for pressure vessels

Stainless steel forgings for pressure vessels

Chemical composition(wt.%) of STSF316 grade: to D 4115 (2001)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.040
S - 0.030
Cr 16.00 18.00
Ni 10.00 14.00
Mo 2.00 3.00

STSF316 - Detail

Stainless steel forgings for pressure vessels

Mechanical properties of grade STSF316 D 4115 (2001)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
772 (≥) 941 (≥) 21 23 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade STSF316 D 4115 (2001)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
197 (≥) 168 (≥) 11 22 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
172 951 248