STSF316H Stainless Steels to D 4115 (2001)

STSF316H - Specification & Application

  • D 4115 (2001) - Stainless steel forgings for pressure vessels

Stainless steel forgings for pressure vessels

Chemical composition(wt.%) of STSF316H grade: to D 4115 (2001)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 2.00
P - 0.040
S - 0.030
Cr 16.00 18.00
Ni 11.00 14.00
Mo 2.00 3.00

STSF316H - Detail

Stainless steel forgings for pressure vessels

Mechanical properties of grade STSF316H D 4115 (2001)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
682 (≥) 571 (≥) 23 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade STSF316H D 4115 (2001)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
669 (≥) 711 (≥) 31 33 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
819 349 823

Equivalent Grade

Equivalent Products