STSF321H Stainless Steels to D 4115 (2001)

STSF321H - Specification & Application

  • D 4115 (2001) - Stainless steel forgings for pressure vessels

Stainless steel forgings for pressure vessels

Chemical composition(wt.%) of STSF321H grade: to D 4115 (2001)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 2.00
P - 0.040
S - 0.030
Cr 17.00 20.00
Ni 9.00 13.00
Mo - -
Ti 4×C% 0.60

STSF321H - Detail

Stainless steel forgings for pressure vessels

Mechanical properties of grade STSF321H D 4115 (2001)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
961 (≥) 456 (≥) 23 14 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade STSF321H D 4115 (2001)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
569 (≥) 955 (≥) 12 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 342
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
983 322 262