Chemical composition(wt.%) of STSF410B grade: to D 4115 (2001)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 11.50 13.50
Ni - 0.60
Mo - -

STSF410B - Detail

Stainless steel forgings for pressure vessels

Mechanical properties of grade STSF410B D 4115 (2001)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
159 (≥) 138 (≥) 22 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade STSF410B D 4115 (2001)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
255 (≥) 569 (≥) 21 41 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
518 524 994