SUH36 Stainless Steels

SUH36 - Specification & Application

CNS standard heat resistant steel bar steel grade and chemical composition

Chemical composition(wt.%) of SUH36 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.48 0.58
Si - 0.35
Mn 8.00 10.00
P - 0.040
S 0.04 0.09
Cr 20.00 22.00
Ni 3.25 4.50
Mo - -
N 0.35 0.50

SUH36 - Detail

CNS standard heat resistant steel bar steel grade and chemical composition

Mechanical properties of grade SUH36

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
852 (≥) 767 (≥) 31 34 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade SUH36

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
211 (≥) 158 (≥) 32 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
733 484 831

Equivalent Grade

Equivalent Products

We can customize the production of SUH36 grade, contact us for the best solution.