SUH38 Stainless Steels

SUH38 - Specification & Application

CNS standard heat resistant steel bar steel grade and chemical composition

Chemical composition(wt.%) of SUH38 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.25 0.35
Si - 1.00
Mn - 1.20
P 0.18 0.25
S - 0.030
Cr 19.00 21.00
Ni 10.00 12.00
Mo 1.80 2.50
N - -
B 0.001 0.010

SUH38 - Detail

CNS standard heat resistant steel bar steel grade and chemical composition

Mechanical properties of grade SUH38

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
453 (≥) 434 (≥) 31 11 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade SUH38

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
651 (≥) 797 (≥) 12 33 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
971 674 353

Equivalent Grade

Equivalent Products

We can customize the production of SUH38 grade, contact us for the best solution.