Chemical composition(wt.%) of SUH409 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 10.50 11.75
Ni - 0.60
Mo - -
Ti 6×C% 0.75

SUH409 - Detail

CNS standard heat resistant steel plate of the steel grade and chemical composition

Mechanical properties of grade SUH409

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
617 (≥) 113 (≥) 31 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade SUH409

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
732 (≥) 783 (≥) 11 22 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
735 431 931