SUH661 Stainless Steels

SUH661 - Specification & Application

CNS standard heat resistant steel bar steel grade and chemical composition

Chemical composition(wt.%) of SUH661 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.20
S - 0.15
Cr 17.00 19.00
Ni 8.00 10.00
Mo - 0.60
N - -
Co 18.50 21.00
W 2.00 3.00
Nb 0.75 1.25

SUH661 - Detail

CNS standard heat resistant steel bar steel grade and chemical composition

Mechanical properties of grade SUH661

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
111 (≥) 691 (≥) 32 34 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade SUH661

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
871 (≥) 753 (≥) 23 33 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
314 312 718