Chemical composition(wt.%) of SUS XM7 grade: to G 4303 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 17.00 19.00
Ni 8.50 10.50
Mo - -
N - -
Cu 3.00 4.00

SUS XM7 - Detail

Stainless steel bars

Mechanical properties of grade SUS XM7 G 4303 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
986 (≥) 889 (≥) 22 34 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade SUS XM7 G 4303 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
358 (≥) 954 (≥) 23 11 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
265 688 563