T11344 Tool Die Steels

T11344 - Specification & Application

High-Speed Tool Steel

Chemical composition(wt.%) of T11344 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.10 1.20
Si 0.30 0.55
Mn 0.20 0.40
P - 0.030
S - 0.030
Cr 4.00 4.75
Mo 6.00 7.00
V 1.85 2.20
W 5.00 5.75
Co 11.00 12.25

T11344 - Detail

High-Speed Tool Steel

Mechanical properties of grade T11344

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
732 (≥) 619 (≥) 32 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade T11344

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
266 (≥) 862 (≥) 34 13 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
661 795 477

Equivalent Grade

Equivalent Products

We can customize the production of T11344 grade, contact us for the best solution.
sales@specificsteel.com