T30110 Tool Die Steels

T30110 - Specification & Application

Cold-Work Tool Steel

Chemical composition(wt.%) of T30110 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.25 1.50
Si 1.00 1.50
Mn 1.60 2.10
P - 0.030
S - 0.030
Cr - -
Mo 1.25 1.75
V - -
W - -
Ni+Cu - 0.75
Ni 1.55 2.05

T30110 - Detail

Cold-Work Tool Steel

Mechanical properties of grade T30110

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
299 (≥) 313 (≥) 43 24 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade T30110

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
774 (≥) 132 (≥) 24 14 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
193 717 125

Equivalent Grade

Equivalent Products

We can customize the production of T30110 grade, contact us for the best solution.