T61206 Tool Die Steels

T61206 - Specification & Application

Low Alloy Tool Steel

Chemical composition(wt.%) of T61206 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.65 0.75
Si 0.10 0.50
Mn 0.25 0.80
P - 0.030
S - 0.030
Cr 0.60 1.20
Mo - 0.50
V - -
W - -
Ni+Cu - 0.75
Ni 1.25 2.00

T61206 - Detail

Low Alloy Tool Steel

Mechanical properties of grade T61206

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
187 (≥) 142 (≥) 14 14 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade T61206

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
458 (≥) 298 (≥) 24 34 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
591 925 823

Equivalent Grade

Equivalent Products

We can customize the production of T61206 grade, contact us for the best solution.