Chemical composition(wt.%) of TUZ6CNDT17-12 grade: to NF A 49-117

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.060
Si - 0.75
Mn - 2.00
P - 0.040
S - 0.015
Cr 16.00 18.00
Mo 2.00 2.50
Ni 10.50 12.50
N - 0.020
Ti 5(C+N) 0.70

TUZ6CNDT17-12 - Detail

Steel tubes. Seamless plain end tubes for pipes-lines and other uses. Ferritic and austenitic stainless steels. Dimensions. Technical delivery conditions

Mechanical properties of grade TUZ6CNDT17-12 NF A 49-117

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
767 (≥) 685 (≥) 43 32 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade TUZ6CNDT17-12 NF A 49-117

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
667 (≥) 593 (≥) 42 33 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
318 813 572