U20082 Structural Steel to GB/T 699-1999

U20082 - Specification & Application

  • GB/T 699-1999 - This standard specifies the alloy steel, low alloy steel, alloy steel chemical composition relative to the provisions of the finished steel smelting chemical composition boundary limit allowable deviation, and gives the definition of related terms.
  • GB 13237-1991 -
  • GB/T 13793-1992 -
  • GB 3206-1982 -
  • GB/T 711-2008 -
  • GB 3275-1991 -
  • GB 699-1988 -
  • GB 710-1991 -
  • GB 711-1988 -

This standard specifies the alloy steel, low alloy steel, alloy steel chemical composition relative to the provisions of the finished steel smelting chemical composition boundary limit allowable deviation, and gives the definition of related terms.

Chemical composition(wt.%) of U20082 grade: to GB/T 699-1999

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.11
Si - 0.03
Mn 0.25 0.5
P - 0.035
S - 0.035
Cr - 0.1
Ni - 0.3
Cu - 0.25

U20082 - Detail

Delivery status: hot or hot forging
This standard specifies the alloy steel, low alloy steel, alloy steel chemical composition relative to the provisions of the finished steel smelting chemical composition boundary limit allowable deviation, and gives the definition of related terms.

ReL (MPa) Rm (MPa) Z (%) A5.65 (%) Heat treatment condition Technology Sampl
175(≥) 295(≥) 60(≥) 35(≥) Normalizing 930℃ Heat preservation≥30min AC Normalizing 25(Sampl size)

HBS: 131(≤)


Mechanical properties of grade U20082 GB/T 699-1999

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
277 (≥) 692 (≥) 22 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade U20082 GB/T 699-1999

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
736 (≥) 474 (≥) 31 14 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
325 671 947

Equivalent Products