X10CrMoVNb9-1 Stainless Steels to EN 10302: 2008

X10CrMoVNb9-1 - Specification & Application

  • EN 10302: 2008 - Creep resisting steels, nickel and cobalt alloys
  • EN 10028-2: 2009 - Flat products made of steels for pressure purposes. Non-alloy and alloy steels with specified elevated temperature properties
  • EN 10222-2: 2000 - Steel forgings for pressure purposes. Ferritic and martensitic steels with specified elevated temperature properties
  • EN 10216-2: 2014 - Seamless steel tubes for pressure purposes. Technical delivery conditions. Non-alloy and alloy steel tubes with specified elevated temperature properties
  • EN 10253-2: 2007 - Butt-welding pipe fittings. Non alloy and ferritic alloy steels with specific inspection requirements
  • EN 10088-1: 2005 - Stainless steels. List of stainless steels

Alloy special martensitic creep-resisting steel

Chemical composition(wt.%) of X10CrMoVNb9-1 grade: to EN 10302: 2008

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.12
Si - 0.5
Mn 0.3 0.6
Ni - 0.4
P - 0.025
S - 0.015
Cr 8.0 9.5
Mo 0.85 1.05
V 0.18 0.25
N 0.03 0.07
Nb 0.06 0.10
Al - 0.03

X10CrMoVNb9-1 - Detail

X10CrMoVNb9-1

Mechanical properties of grade X10CrMoVNb9-1 EN 10302: 2008

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
688 (≥) 953 (≥) 11 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade X10CrMoVNb9-1 EN 10302: 2008

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
988 (≥) 367 (≥) 33 12 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
375 679 893

Equivalent Products

We can customize the production of X10CrMoVNb9-1 grade, contact us for the best solution.