X3CrNiCu18-9 3E Stainless Steels to ISO 4954

X3CrNiCu18-9 3E - Specification & Application

  • ISO 4954 - Steels for cold heading and cold extruding

Steels for cold heading and cold extruding

Chemical composition(wt.%) of X3CrNiCu18-9 3E grade: to ISO 4954

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 17.00 19.00
Ni 8.50 10.50
Mo - -
Cu 3.00 4.00

X3CrNiCu18-9 3E - Detail

Steels for cold heading and cold extruding

Mechanical properties of grade X3CrNiCu18-9 3E ISO 4954

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
935 (≥) 238 (≥) 12 41 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade X3CrNiCu18-9 3E ISO 4954

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
697 (≥) 131 (≥) 12 21 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
571 591 884

Equivalent Products

We can customize the production of X3CrNiCu18-9 3E grade, contact us for the best solution.