X55CrMnNiN20-8 Stainless Steels to NF EN 10090

X55CrMnNiN20-8 - Specification & Application

  • NF EN 10090 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of X55CrMnNiN20-8 grade: to NF EN 10090

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.50 0.60
Si - 0.25
Mn 7.00 10.00
P - 0.035
S - 0.030
Cr 19.50 21.50
Ni 1.50 2.75
Mo - -
N 0.20 0.40

X55CrMnNiN20-8 - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade X55CrMnNiN20-8 NF EN 10090

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
315 (≥) 766 (≥) 21 11 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade X55CrMnNiN20-8 NF EN 10090

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
884 (≥) 288 (≥) 33 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
621 573 368

Equivalent Products

We can customize the production of X55CrMnNiN20-8 grade, contact us for the best solution.
sales@specificsteel.com