X63CrMoV5-1 Tool Die Steels

X63CrMoV5-1 - Specification & Application

Alloyed CrMoV steel

Chemical composition(wt.%) of X63CrMoV5-1 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.60 0.65
Si 1.00 1.20
Mn 0.30 0.50
P - 0.035
S - 0.035
Cr 5.00 5.50
Mo 1.00 1.30
V 0.25 0.35
Cu - 0.30

X63CrMoV5-1 - Detail

Alloyed CrMoV steel

Mechanical properties of grade X63CrMoV5-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
855 (≥) 171 (≥) 44 23 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade X63CrMoV5-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
893 (≥) 875 (≥) 44 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
535 434 444

Equivalent Grade

Equivalent Products

We can customize the production of X63CrMoV5-1 grade, contact us for the best solution.