X64CrMo14 Tool Die Steels

X64CrMo14 - Specification & Application

High alloyed CrMo steel

Chemical composition(wt.%) of X64CrMo14 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.60 0.70
Si 0.30 0.50
Mn 0.40 0.60
P - 0.025
S - 0.025
Cr 13.50 14.50
Mo 0.50 0.70
V 0.05 0.15

X64CrMo14 - Detail

High alloyed CrMo steel

Mechanical properties of grade X64CrMo14

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
523 (≥) 941 (≥) 43 24 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade X64CrMo14

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
582 (≥) 736 (≥) 13 32 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
331 528 755

Equivalent Grade

Equivalent Products

We can customize the production of X64CrMo14 grade, contact us for the best solution.