X6CrMo4 Tool Die Steels

X6CrMo4 - Specification & Application

Alloyed CrMo steel

Chemical composition(wt.%) of X6CrMo4 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 0.20
Mn - 0.20
P - 0.030
S - 0.030
Cr 3.50 4.00
Mo 0.30 0.60
V - -

X6CrMo4 - Detail

Alloyed CrMo steel

Mechanical properties of grade X6CrMo4

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
517 (≥) 898 (≥) 24 32 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade X6CrMo4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
845 (≥) 259 (≥) 12 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 222
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
755 268 483

Equivalent Grade

Equivalent Products