X6CrNb12E Stainless Steels to ISO 4954

X6CrNb12E - Specification & Application

  • ISO 4954 - Steels for cold heading and cold extruding

Steels for cold heading and cold extruding

Chemical composition(wt.%) of X6CrNb12E grade: to ISO 4954

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 10.50 12.50
Ni - 0.50
Mo - -
Nb 6×C% 1.00

X6CrNb12E - Detail

Steels for cold heading and cold extruding

Mechanical properties of grade X6CrNb12E ISO 4954

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
141 (≥) 794 (≥) 12 24 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade X6CrNb12E ISO 4954

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
644 (≥) 899 (≥) 22 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
761 789 745

Equivalent Grade

Equivalent Products

We can customize the production of X6CrNb12E grade, contact us for the best solution.