XH38BT Stainless Steels

XH38BT - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH38BT grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.06 0.12
Si - 0.80
Mn - 0.70
P - 0.030
S - 0.020
Cr 20.00 23.00
Ni 35.00 39.00
Mo - -
Al - 0.50
Ti 0.70 1.20
Fe - -
W 2.80 3.50
Ce - 0.05

XH38BT - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH38BT

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
184 (≥) 437 (≥) 14 42 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade XH38BT

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
165 (≥) 427 (≥) 43 43 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
384 433 282

Equivalent Grade

Equivalent Products

We can customize the production of XH38BT grade, contact us for the best solution.
sales@specificsteel.com