Z11CN18.08CI Stainless Steels to NF A 35-595

Z11CN18.08CI - Specification & Application

  • NF A 35-595 - Iron and steel. Cutlery stainless steel

Iron and steel. Cutlery stainless steel

Chemical composition(wt.%) of Z11CN18.08CI grade: to NF A 35-595

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.090 0.12
Si - 0.75
Mn 0.75 1.20
P - 0.040
S - 0.015
Cr 16.50 18.50
Mo - -
Ni 7.00 8.00

Z11CN18.08CI - Detail

Iron and steel. Cutlery stainless steel

Mechanical properties of grade Z11CN18.08CI NF A 35-595

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
372 (≥) 147 (≥) 32 33 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade Z11CN18.08CI NF A 35-595

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
264 (≥) 114 (≥) 23 31 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 242
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
897 296 897

Equivalent Products

We can customize the production of Z11CN18.08CI grade, contact us for the best solution.
sales@specificsteel.com