Z12CND16-04 Air 9160/C Aviation and Aero Steel to AIR 9160 C

Z12CND16-04 Air 9160/C - Specification & Application

  • AIR 9160 C - wrought steels used in aeronautical constructions

wrought steels used in aeronautical constructions

Chemical composition(wt.%) of Z12CND16-04 Air 9160/C grade: to AIR 9160 C

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 0.50
Mn 0.70 1.30
P - 0.035
S - 0.025
Cr 15.00 16.00
Ni 4.00 5.00
Mo 2.50 3.25
N 0.05 0.15
Cu - 0.20

Z12CND16-04 Air 9160/C - Detail

Z12CND16-04 Air 9160C wrought steels used in aeronautical constructions

Mechanical properties of grade Z12CND16-04 Air 9160/C AIR 9160 C

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
197 (≥) 317 (≥) 43 33 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade Z12CND16-04 Air 9160/C AIR 9160 C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
616 (≥) 842 (≥) 33 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
762 717 752

Equivalent Grade

Equivalent Products

We can customize the production of Z12CND16-04 Air 9160/C grade, contact us for the best solution.