Z12CND16-05-03 Stainless Steels to NF A 35-574

Z12CND16-05-03 - Specification & Application

  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Chemical composition(wt.%) of Z12CND16-05-03 grade: to NF A 35-574

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.080 0.15
Si - 0.50
Mn 0.70 1.30
P - 0.035
S - 0.025
Cr 15.00 16.00
Mo 2.50 3.25
Ni 4.00 5.00
Cu - 0.20
N 0.05 0.15

Z12CND16-05-03 - Detail

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Mechanical properties of grade Z12CND16-05-03 NF A 35-574

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
447 (≥) 317 (≥) 41 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade Z12CND16-05-03 NF A 35-574

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
396 (≥) 865 (≥) 14 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
472 687 568

Equivalent Products

We can customize the production of Z12CND16-05-03 grade, contact us for the best solution.