Z15CN16-02 Stainless Steels to NF A 35-574

Z15CN16-02 - Specification & Application

  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod
  • NF F 80-109 - Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Chemical composition(wt.%) of Z15CN16-02 grade: to NF A 35-574

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.20
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.025
Cr 15.50 17.00
Mo - -
Ni 1.50 2.50

Z15CN16-02 - Detail

Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Mechanical properties of grade Z15CN16-02 NF A 35-574

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
179 (≥) 225 (≥) 31 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade Z15CN16-02 NF A 35-574

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
389 (≥) 823 (≥) 34 31 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 223
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
796 815 314