Z20CN21-12Az Stainless Steels to NF A 35-579

Z20CN21-12Az - Specification & Application

  • NF A 35-579 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of Z20CN21-12Az grade: to NF A 35-579

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.25
Si 0.70 1.30
Mn 1.00 1.50
P - 0.040
S - 0.030
Cr 20.00 22.00
Ni 10.50 12.50
Mo - -
N 0.15 0.25

Z20CN21-12Az - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade Z20CN21-12Az NF A 35-579

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
397 (≥) 359 (≥) 13 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade Z20CN21-12Az NF A 35-579

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
899 (≥) 741 (≥) 32 42 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
685 593 881

Equivalent Grade

Equivalent Products

We can customize the production of Z20CN21-12Az grade, contact us for the best solution.