Z21CDNbV11 Stainless Steels to NF A 35-578

Z21CDNbV11 - Specification & Application

  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application

Iron and steel. Stainless steel for high temperature application

Chemical composition(wt.%) of Z21CDNbV11 grade: to NF A 35-578

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.16 0.25
Si 0.10 0.50
Mn 0.30 0.80
P - 0.030
S - 0.015
Cr 10.00 12.00
Mo - 1.00
Ni 0.50 1.00
Nb 0.25 0.55
V 0.10 0.30
N 0.05 0.10

Z21CDNbV11 - Detail

Iron and steel. Stainless steel for high temperature application

Mechanical properties of grade Z21CDNbV11 NF A 35-578

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
398 (≥) 951 (≥) 34 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade Z21CDNbV11 NF A 35-578

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
519 (≥) 113 (≥) 32 23 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
316 268 339

Equivalent Grade

Equivalent Products

We can customize the production of Z21CDNbV11 grade, contact us for the best solution.
sales@specificsteel.com