Z25CNWS20-09 Stainless Steels to NF A 35-579

Z25CNWS20-09 - Specification & Application

  • NF A 35-579 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of Z25CNWS20-09 grade: to NF A 35-579

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 0.30
Si 0.75 1.50
Mn - 2.00
P - 0.040
S - 0.030
Cr 19.50 21.50
Ni 8.50 10.50
Mo - -
N 0.15 0.25

Z25CNWS20-09 - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade Z25CNWS20-09 NF A 35-579

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
825 (≥) 695 (≥) 33 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade Z25CNWS20-09 NF A 35-579

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
354 (≥) 264 (≥) 34 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
248 193 122

Equivalent Grade

Equivalent Products

We can customize the production of Z25CNWS20-09 grade, contact us for the best solution.