Z29CF13 Stainless Steels to NF A 35-574

Z29CF13 - Specification & Application

  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Chemical composition(wt.%) of Z29CF13 grade: to NF A 35-574

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.25 0.32
Si - 1.00
Mn - 1.50
P - 0.040
S 0.15 0.25
Cr 12.00 13.50
Mo - 0.60
Ni - 0.75

Z29CF13 - Detail

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Mechanical properties of grade Z29CF13 NF A 35-574

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
122 (≥) 589 (≥) 43 21 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade Z29CF13 NF A 35-574

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
625 (≥) 977 (≥) 12 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
635 287 679

Equivalent Grade

Equivalent Products

We can customize the production of Z29CF13 grade, contact us for the best solution.
sales@specificsteel.com