Z3CN19-09 Stainless Steels to NF A 35-574

Z3CN19-09 - Specification & Application

  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Chemical composition(wt.%) of Z3CN19-09 grade: to NF A 35-574

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 0.75
Mn - 2.00
P - 0.040
S 0.015 0.030
Cr 18.00 19.00
Mo - -
Ni 8.00 10.00

Z3CN19-09 - Detail

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Mechanical properties of grade Z3CN19-09 NF A 35-574

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
646 (≥) 656 (≥) 42 34 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade Z3CN19-09 NF A 35-574

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
643 (≥) 121 (≥) 23 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
173 217 978

Equivalent Grade

Equivalent Products

We can customize the production of Z3CN19-09 grade, contact us for the best solution.